dc.description.abstractMaritime pine (Pinus pinaster) wood has low dimensional stability and durability. Heat treatment was made in an oven using hot air during 2 to 24 h and at 170-200 ÂșC. A comparison was made against steam heat treatment. The equilibrium moisture content and the dimensional stability (ASE) in radial and tangential directions were evaluated at 35%, 65% and 85% relative humidity. MOE, bending strength and wettability were also determined. At the same mass loss improvements of equilibrium moisture content and dimensional stability were higher for oven heat treatment but the same happened for mechanical strength degradation. A 50% decrease in hemicellulose content led to a similar decrease in bending strength.por
dc.identifier.citationEsteves, B. M., Domingos, I. J., and Pereira, H. M. 2008. Pine wood modification by heat treatment in air, BioRes. 3(1), 142-154.por
dc.identifier.urihttp://hdl.handle.net/10400.19/1079
dc.language.isoengpor
dc.peerreviewedyespor
dc.subjectHeat treatmentpor
dc.subjectwood modificationpor
dc.titlePine wood modification by heat treatment in airpor
dc.typejournal article
dspace.entity.typePublication
oaire.citation.endPage154por
oaire.citation.startPage142por
oaire.citation.titleBioresourcespor
rcaap.rightsopenAccesspor
rcaap.typearticlepor

Ficheiros

Principais
A mostrar 1 - 1 de 1
Miniatura indisponĂ­vel
Nome:
Pine wood modification by heat treatment in air -Bio RIPV.pdf
Tamanho:
256.63 KB
Formato:
Adobe Portable Document Format
Licença
A mostrar 1 - 1 de 1
Miniatura indisponĂ­vel
Nome:
license.txt
Tamanho:
1.71 KB
Formato:
Item-specific license agreed upon to submission
Descrição: